Tanning is the process of making leather from skin. This is commonly done with the acidic compound tannin, which prevents normal decomposition and often imparts color.

  • Metonymically, like hiding, tanning may also refer to any corporal punishment (e.g. paddling, whipping, as in the expression 'to tan one's hide'), hard enough to clearly colour (usually bright red, or even purple, later often 'black and blue') the painfully beaten skin of the victim.

Process

The process of dressing up animal skin/hide into leather consists of three stages. The first stage is the preparation for tanning. The second stage is the actual tanning and other chemical treatment. The third stage applies finishing to the surface.

In preparation for tanning, the skins (of smaller animals like goat, sheep, lamb, pig, etc) or hides (of larger animals like cow, buffalo, etc) are washed, treated with lime/sulfide to remove hair and natural fat, then delimed to remove sulfide and acidified to prepare for tanning.

The majority of leather produced today is tanned using chromeIII tanning material.In the raw state chrome tanned skins are blue and therefor referred to as "wet blue". The wet blue is then split for the desired end product, garment upholstery, shoe upper etc, followed by dyeing (to give color), fatliquoring (to add fat/oil) and retanning (to fill up the fiber structure) in wet condition.

The leathers are dried and mechanically softened and prepared for finishing. Finishing is usually done by coating the surface with paint-like mixes. Suedes, Nubucks, etc. are finished by raising the nap of the leather by rubbing with emery paper (sandpaper).

Another process, that was used by Native Americans, involves "tanning" the skin using brains. First, the hide can be strung in a frame. Second, the flesh from skins is scraped as before. Then the hide is allowed to dry after which the hair on these skins is shaved off. Then, brains are mixed with a minimum of water. The hide soaks for 24 hours. Then, you stretch it as it dries. Finally, you sew the skin in a bag and smoke it using rotten wood placed on coals.

History of Tanning

In ancient history, tanning was considered a noxious trade and relegated to the outskirts of town, amongst the poor. The ancients used leather for waterskins, bags, harnesses, boats, armor, quivers, scabbards, boots, and sandals. Around 2500 BC, the Sumerians began using leather, affixed by copper studs, on chariot wheels.

Tanners would take an animal skin and soak it in water. Then they would pound and scour the skin to remove flesh and fat. Next, either they soaked the skin in urine to loosen hair fibers or they let the skin putrefy for several months, after which they dipped the skin in a salt solution. After the hair fibers were loosened, the tanners would scrape them off with a knife.

Once the hair was removed, tanners would bate the material by pounding dung into the skin or soaking the skin in a solution of animal brains. They would also take cedar oil, alum, or tannin and stretch the skin as it lost moisture and absorbed the tanning agent.

Leftover leather would be turned into glue. Tanners would place scraps of hides in a vat of water and let them deteriorate for months. The mixture would then be placed over a fire to boil off the water to produce hide glue.